Showing posts with label Epoxy. Show all posts
Showing posts with label Epoxy. Show all posts

Wednesday, July 10, 2013

Experimenting with Xynole -- 374 hours

I got the idea of using Xynole from David at BoatSmith, he is a professional Wharram builder down in Jupiter Florida. He had told me once in a conversation that he used Xynole on the hull exterior instead of FG as called for in the plans. Also on the RAKA site they call Xynole the poor man's Kevlar.  It's supposed to have much higher impact and abrasion resistance than fiberglass.
So in with my last epoxy order I bought a couple yards of 68ich wide 4oz  Xynole. It was $8.75/ydr compared to $6.50/ydr for 60inch wide 4oz plain weave fiberglass cloth.

My test spot was in the stern buoyancy compartment below the stiffener, a small triangular area. I wanted to observe the wet-out up close and make sure the wet-out was thorough. So first I cut a pattern using craft paper then cut the Xynole and did the wet-out on my plastic covered work bench.  I found out it really soaks up the epoxy. It seemed to use 2 or 3 times the amount of epoxy than my 12oz FG biaxial tape. Next the transfer from bench to hull was tricky since the cloth stretches and flops around easily due to the open weave.
Stern buoyancy compartment, Xynole experiment. 
I think it's obvious this is not the material to use for a clear coat:) Above the stiffener the plywood has just 2 coats of epoxy and sanded. Oh well, this is why I did my experiment in the bottom of the buoyancy compartment, a place only viewed by serious contortions. But should there ever be a puncture event in this area, the Xynole will deflect and absorb the hit and hopefully keep water from entry. I'm debating if I should use the Xynole on the interior of the bow buoyancy compartment, this is the area most likely to encounter some mysterious object in the middle of the ocean in the middle of the night.

I should note that I've planned not to paint the buoyancy compartments and other lower areas of the hull. I don't ever want creeping wood rot hiding behind paint. If there is a problem, I'd rather see it earlier than later.




Monday, July 8, 2013

Keel Fillets and glassing DONE!!! -- 373 hours


From Stem to 

Stern. 
Not really too much picture worthy with this work, just pouring epoxy to a uniform level in the 7 distinct keel compartments from stem to stern. The front four were actually much easier to get done since I was able to lift the rear of the hull to get the three front compartment keel areas close to level. This made it easy to pour a less thick mixture and let it self level. The rear three compartments took longer since lifting the front wasn't as straight forward as lifting the back. The skeg is only a few cm off the floor so really to get the rear near level the whole hull forward of the skeg needs to be lifted. This seemed too hard, so instead I used thicker mixtures and made small dams about 15cm apart. Then I'd pour a thinner mixture in between, creating steps that then were filled with thicker mixtures. This worked pretty well between bulkheads 4/6 and 6/7.  But from bulkhead 7 to the stern post the buoyancy compartment swings upward quickly so mostly very thickened epoxy is needed to stick to the near vertical gaps.

I feel like I've had a pretty good run this past month but it's time to throttle back on Tiki work and  put more time in to other household projects e.g. crack repairs.  After a minor earthquake last October we had several hairline cracks on the SW dome face. We didn't realize it until this spring when we got back from our southern vacation. So I've started cleaning and caulking, but many hours ahead since we also decided to change house colors.

Tuesday, July 2, 2013

Don't let this happen.... -- 353 hours

It takes a lot of epoxy to fill the keel and attach stringers/stiffeners so don't do like I did and wait until you start the last gallon bottle of epoxy resin to order your next batch from your favorite supplier:(

The issue is that I have several, what I call, "wet edges" of epoxy kicking and I'm very low on epoxy and about to run out.

With epoxy I use the term "wet edge" (which is from painting) for the time period after pouring during which when new epoxy is poured and it will still chemically bond with the first pour. The type of hardener, the ambient temperature, and volume of epoxy all combine to set the wet edge time frame.

The temperature in my basement is about 72degF and dropping slightly. This past week has been cool and wet here in Maine, for instance today we had a high temp of about 61degF. And I'm using RAKA 606 slow hardener so the wet edge period is about 24 hrs. Around this time the bond becomes less and less chemical and more mechanical until after about a week when it has completely kicked. The point being I what to keep that chemical bond going as it is much stronger than the mechanical bond.  Also after this wet period is when amine blush can develop, although luckily I have virtually no issues with blush at this site.

Lower hull stringers between bulkhead 3 and 4.
A little tip to help spread the hull when installing stringers/stiffeners. First dry fit the port and starboard pieces. I use two screws on each piece to hold the stringer. Then using two pieces of wood with notches over lap them and use safety wire to hold them together. Then using a screw clamp its easy to carefully adjust the spread to get the desired "fair" curve of the hull.

Sunday, June 30, 2013

What feels like real progress -- 343 hrs

The couple pics don't look like much has changed but at this point the keel is about 57% poured and glassed. The keel is complete from the stem to bulkhead 4 and started from BH4 to stern post. Also bulkheads 1,2,3, and 4 are properly filleted in place to the height needed at this stage. This stage of the build is epoxy intensive, I've gone through 4 gallons of epoxy, 5 or 6 pounds of hardwood flour and a couple yards of 12oz biaxial 6inch wide fiberglass tape. In total I've used up about 15 gallons of epoxy since the beginning of the Tiki build. But not all of that was used on the Tiki. Last spring I built a Tear Drop camper and dipped in to my epoxy stash a bit:)

I also finished off my supply of Douglas Fir making the lower hull stringers. After installing the bow buoyancy compartment stiffeners I modified the way I make the stringers/stiffeners. When installing the port and starboard stringers/stiffeners are pushed outward to give the hull a fair curve. Well this puts quite a bit of pressure on the stringer/hull side joint and forces a lot of the epoxy out of the joint. Epoxy joints are supposed to have only light clamping pressure or else a weak "dry joint" will result.
The bow stiffeners wedged apart to give the proper curve.

Completed bow with extra fillets on the stiffeners.

Modified stringers/stiffeners.
I used the router table with a 1/2" mortise bit to cut the epoxy channel. 




Monday, June 24, 2013

2 parts resin+1 part hardener, mix 1 min, add wood flour as needed, repeat.......... 305hrs

Epoxy Table, I'm spending a lot of time standing here:)
The title about sums up what I've been doing the past few days and it looks like what I'll be doing for the next few days. With the measuring cups, mixing cups and other stuff it seems a 3/4 cup per mix is about optimum, especially when using fast hardener. I would like to mix larger amounts but with the weather warming up, 75degF in the basement, the Fast hardener is too fast. It starts to kick in about 10-15 minutes, heck it becomes warn to the touch in the cup before I can walk from the epoxy table to the boat. So I have to be ready to spread it out quickly to slow down the reaction. Using the slow hardener extends the initial cure time to 2-3 hours. Thats great for working it but I then have to remember to come back to smooth the fillets, like on the bulkheads, later before it kicks hard and be careful not to get a wayward elbow in a soft fillet:)
An early pour.

Bow, stem area. Keel timber finished with fiberglass, stem still
needs more epoxy build up.